產(chǎn)品詳情
Grade : 1.4713鐵素體耐熱鋼
Number: X10CrAlSi7
Classification: 鐵素體耐熱鋼
Density: 7.7 g/cm 3
Standard:
EN 10095:1999耐熱鋼和鎳合金
EN 10088-1:2005不銹鋼。不銹鋼清單
Equivalent grades:
Chemical comb % of steel X10CrAlSi7 (1.4713): EN 10095-1999
C
|
Si
|
Mn
|
P
|
S
|
Cr
|
Al
|
max 0.12
|
0.5 - 1
|
max 1
|
max 0.04
|
max 0.015
|
6月8日
|
0.5 - 1
|
Mechanical properties of steel X10CrAlSi7 (1.4713)
|
|
|
|
Rm - Tensile strength (MPa) (+A)
|
420-620
|
|
|
|
|
Rp0.2 0.2% proof strength (MPa) (+A)
|
220
|
|
|
|
|
A - Min. elongation at fracture (%) (+A)
|
15-20
|
|
|
Brinell hardness (HB): (+A)
|
192
|
Properties of steel X10CrAlSi7 (1.4713)
|
|
Maximum application temperature for air T= 800 ° C
|
|